Quote:
|
Originally Posted by lfsracing
Just wondering does anyone know where to get some good high temp ceramic powder? Looking to coat some exhaust pieces and turbo pieces that can get really close to 1600 degrees. The current turbo setup on one of my cars puts out close to 1600 EGT's which is quite hot. I know they make stuff to do temps this hot and just don't want to risk coating something with the high temp powders that I seen on caswells site without knowing they will be able to handle it. Any help would be great. Hopefully this is something caswell would consider getting in as I need to order some things already so would just add this to my list.
Lorenzo
|
Lorenzo,
There is no such thing as High Temp Ceramic Powder, the ceramic coat is a wet product. As RNMHRD said look for Tech line coatings, I use then all the time. You will need an oven that reaches a min temp of 500 degrees..
Jim S...