Thread: I don't get it
View Single Post
  #1 (permalink)  
Old 10-08-2006, 05:22 PM
blewis999 blewis999 is offline
Newbie
 
Join Date: Sep 2006
Posts: 21
blewis999 is on a distinguished road
Default I don't get it

I am on my second batch. This is fun. But I thought the voltage (as read on my cc/cv display should increase as time goes on.

My first batch was 41in^2 set to 1.7A for 120min. Voltage started around 16V then fell as time went on. ended around 14.5 or something.

Parts turned out great.

Second batch : 71 in^2 set to 3A for 120 min. Valtage started at 15.1 Now half way through it is 13.9.

Am I thinking backwards?
Reply With Quote