Shawn
I’d like to see the piece you are talking about . Im also wandering if you are putting any thing to protect the part after plating and then again about three weeks later should use a once a year car polish or collinite metal wax or if maybe your plate was not thick enough or if this was a part you did while your tank was contaminated lots of questions here give ma call if I can help