Quote:
|
Originally Posted by bigkidneys
I apologize if this is in the wrong forum. I recently purchased some B9 nickel stripper to remove the nickel layer from a set of golf club irons I have in order to allow them to rust. I have performed the procedure twice, the heads get the black nickel smut but once i remove the smut by sanding with a dremel tool, the nickel is still there. I am not sure what type of nickel it is. Am I doing something wrong? Please help...
Jason
|
Can you be more specific on your procedure how long are you leaving them in the solution ect.