View Single Post
  #2 (permalink)  
Old 10-16-2006, 11:41 PM
Banditperformance Banditperformance is offline
Metal Finishing Guru
 
Join Date: Jun 2006
Posts: 619
Banditperformance is on a distinguished road
Default Re: powder coating wood??????

I have read that you can PC wood. But, you need to match the PC cure temp to the wood, have enough humidity in the wood to make it conductive to hold the charge etc. Alot of IKEA furniture is PC'd, that I know.
__________________
Dan Pesonen
Bandit Powder Coat <<From Powder to Perfection>>
Forest Grove, BC Canada

Personal motto:
"If it ain't broke, modify somethin till it is"