Re: Weber 40 IDL die cast body finish
Well I know that stromberg is actually still manufacturing carbs out of England in fact I plated one of there brand new out of the box 97s and posted it on this site in my research of this company I have found that any coating put on these carbs has been by a rebuilder not the manufacturer