Quote:
|
Originally Posted by engineerscott
Looks like we will be casting these parts from either A360 or A380. These alloys are in the 8 to 10% Si range. I guess we'll just have to try a few samples with we get first articles back.
Thanks,
|
Good Luck on this, if it works out please tell me I have had an enquiry recently for anodizing castings also but said we couldnt do it. I even rang a few guys up in Australia also about it, they also said no. Maybe the shiney anodize cannot be done