stripper
hey peoplezz..been awhile..found this neat little trick this summer working on my vette...this will degrease and strip paint and even powder coated stuff...depending upon the size part....i used an old metal barrel...good old crystal drano....not the liquid...just mix with some water and let errr soak..i agitated mine with one of those long paint mixer rods that fit on a drill.sure cleaned up the parts sweet...just for laughs i dropped in some stuff i had pc and the powder peeled right off...dont remember how long it took...but it was faster than blasting...