Quote:
|
Originally Posted by seanc
[*]Your bath temp may be too high. Temp range for the original formula is 60-90º. 60's a bit too cold, but 70-80 works good for me.
|
Is there a faster/better way to heat up the bath than with the aquarium heater? Like could this be done in a large crock pot or roaster? Something that heats up faster. I had my heater in my small 2 gal bucket (insulated) for 5 hours and it went up from 60 to 64 degrees. Meanwhile the degreasser went from 60 to 190 in 3 hours in a crock pot.