Neil:
Quote:
|
Is there a faster/better way to heat up the bath than with the aquarium heater? Like could this be done in a large crock pot or roaster?
|
I don't know for sure, but I would not use anything but the compatible plastics. Being an acid, it may react adversely w/ceramics.
Quote:
|
I had my heater in my small 2 gal bucket (insulated) for 5 hours and it went up from 60 to 64 degrees.
|
You've either got a defective heater, or too little wattage.
I use a 200w aquarium heater, and it will bring 3 gallons (uninsulated) from 60 to 100º in about an hour.