Default Re: cheap excellent material for oven walls

i am not building an oven, but wanted to comment. I was using a track torch to cut some 1/4 inch steel diamond plate. The plate was already in place, so 3 inches under needed to be protected. the hardi backer worked for 20 feet of direct oxy torch 3 inches above.

Don't know if this helps, just my experance.