Default Re: Color Sealing???

I've heard of that being done.
Some guys swear that steam sealing/boiling in plain water does not protect against chemicals as well as the nickel acetate sealer, but I have no first hand knowledge of that. If so, I suspect the same with boiling in dye.
__________________
Specializing in anodized graphics in Paintball guns.