A spray bottle with water is handy for cleaning up after the day's use. Also, Acetone will melt and disolve uncured powder real easy. I use water or Acetone to clean my powder cups after the days work, and spray mu gun thourally inside and out with water(with the power off) I don't spray inside the trigger, just the outside, and inside the powder delivery section. It's a good idea to do it at the end of the day, so you sure it will have time to dry before the next time you use it. I am currently trying to rig up a high voltage plug I can use on my gun, so I can remove it form the Pwr supply and take to the sink. Much easier to clean and store then.
__________________
Dan Pesonen
Bandit Powder Coat <<From Powder to Perfection>>
Forest Grove, BC Canada

Personal motto:
"If it ain't broke, modify somethin till it is"
Reply With Quote