Default Re: cheap excellent material for oven walls

It only took 3 1/2 sheets of 18g galv 4 x 10 to do the interior of my 4 x 4 x 4 oven. With a good amount of excess metal for a smaller oven. A little pricey, but I think the product will last longer. One of those; "Way the cost of initial expense vs repeated expense". Just my 2 pennies