Thanks Alalbama. Might hane to give the greaseless a try.
One other question....When I self taught myself to polish, I learned using treated airways. But, as theu lose diameter, they get softer and lose their cutting action. I recently had purchased some spiral sewn from caswell to try and gave them a go this weekend. I like them better...they seem to give a more even cut. But...as they wear down, what happens, do they just eat thru the layer of spiral stitching or what??