View Single Post
  #4 (permalink)  
Old 10-25-2006, 05:55 PM
bzer1 bzer1 is offline
Experienced Metal Finisher
 
Join Date: Jan 2004
Posts: 277
bzer1 is an unknown quantity at this point
Default Re: powder coating a bike engine

Your cure temp and dwell will be manufacturer recommended. Please keep in mind that those temps are part temp NOT oven temp. You start the timer when the part reaches cure temp. For this you will need an IR temp probe. Make sure that you have all the oil residue cleaned off before you apply your powder.