Okay....so been a while...but here are a few pic's of the results from the first few tester parts using e/chrome.
Pre-heated to about 430f then let cool to about 250f then coated then gradually took back up to 392 for 30 mins...
this is just e/chrome with no clear as of yet....
Do they look about right...?
Having some trouble with orange peel and what looks like misting (bit like a white layer underneath....)
Also is it a good idea to use another powder underneath to give the e/chrome depth?....Say black or a dark colour?