Re: Powder coating motorcycle eng.
ALL the old coatings need to be taken off, Media blasting is the best for acheving a uniform, smooth finish with great adhesion. You need to COMPLETELY tear the engine apart too. No seals, bearing's, nothin that cant handle 400*
|