View Single Post
  #1 (permalink)  
Old 10-28-2006, 04:08 AM
albie albie is offline
Newbie
 
Join Date: May 2005
Posts: 4
albie
Default plug n plate silver kit

im having a problem with my plug n plate kit im trying to plate small copper pieces , im using the submerging tecnique the problem is the plating isnt thick enough to be handled, and when i leave the part in longer it turns black and to clean the part it rubs off some silver showing the copper.. i tried alot of things but im out of luck.. would using caswells bigger silver plating kit work better? im thinking about the 1.5 gallon kit you sell especially if it will leave a thicker coating of silver on the parts? any suggestions? thanks albie