How are you cleaning the copper?
How are you cleaning the silver plate after it's plated?
The PNP kits are designed as brush platers. In a pinch, they work for immersion, but immersion plating really requires an adjustable amperage power supply. I would think you'll have better luck sticking to brush plating with the kit.
|