View Single Post
  #1 (permalink)  
Old 11-07-2006, 10:03 PM
MrPontiac MrPontiac is offline
Amateur Metal Finisher
 
Join Date: Aug 2006
Posts: 179
MrPontiac is on a distinguished road
Default Help i don,t understand this part

First off, super, i used the heaters up to 140 degrees and soaked my parts for 30 min. In my other tank i have both plates in with a jumper in between to get positive to both plates, got the heater in distilled water, added chromate crystals then about 1 1/2 teaspoons of yellow brightener, for 30 min. my part is suspened off a 1/2 copper pipe with copper wire, for 30 min. so nothing i see nothing happeneing?? My question maybe i should use just yellow brightener and no crystals, directions are not helpfull