Okay, here's a link to a paper by Lincoln Welders on the subject of carbon precipitation in stainless. Go to section 3.3, which is titled Austentic Stainless Steels, which I certainly assume yours is. Section 3.3.1 is entitled Sensitization. See if that fits your case.
http://content.lincolnelectric.com/p...ure/c64000.pdf