Re: Rust on Stainless Steel
Richard - The rust is just starting to pop in many random areas. It could be poping up like that because of carbon steel contamination or by not getting a thick enough coating of Permalac onto the gate before it was installed.
I'm going to the Lincoln weld site now to read the paper you suggested.
Thanx for your help on this...this whole issue has been very upsetting.
|