View Single Post
  #1 (permalink)  
Old 11-13-2006, 10:44 PM
68commando 68commando is offline
Newbie
 
Join Date: Aug 2006
Posts: 20
68commando is an unknown quantity at this point
Default Copy Chrome questions

I have been using the PNP copy chrome kit for a while now. If you look at the picture, there is a rough plated area above and to the left of the hole in this item. Why is this happening? Could it be lack of cleaning

Also, I have been plating things for about 5 minutes per the instructions using the dip plating instead of the brush plating and now I have upped the time to 1/2 hour to be like the big kits. I noticed that some of the parts I only plated for 5 minutes were rusting and have uneven plating on them. Should I be plating for 5 minutes or 1/2 hour?

Thanks,
Dave
Attached Thumbnails
copy-chrome-questions-img_0007.jpg  
Reply With Quote