Quote:
|
Originally Posted by carrera1984
This was said by the Caswell President-
"Good point. The color panels we have received from our suppliers in the past can differ dramtically from the actual colors when shot over differing metals or bases.
These color chips that everyone wants can be very misleading...which is yet another reason that we don't want to get into selling them."
|
Well with that said, What I shoot and how you shoot we will get 2 different colors as well. So I guess it would be the same thing. Only way you get the same thing over and over again is to shoot a Factory line where everything is 100% the same. Heck color batches change from 1 to the other so no nothing is 100% the same but these are at least a Base to start with..
But hey what do I know I've only been doing this for years. Well you folks do as you like, guess I'm out of here.
Happy Powdering...
Jim S...