I decided to find out what would happen if you powder coat a base color, cure, then airbrush on top, then powder clear. Don't laugh at my airbrushing skills. The first one turned out good with no problems. The second one is supposed to be blue in the center and kinda bled the colors together and cooked. I'm not sure if it was the color or if it was the fact that I put it on alot heavier. I'll do some more when I get time. Has anyone else toyed with this?