Default Yellow chromate mix?

Hi

I just bought a CopyCad kit, 11 liters. I have a few questions I cat find the answers to in the instruction manual:

What is the mixture between destilled water and the yellow chromate? In my kit there was on box with 200 grams of yellow chromate.

Do I need to heat the yellow chromate solution?

In my kit there is a rectifier that is adjustable from 1,5 volts to 12 volts, and it has an output of 500 Milliamps. I have read that 1,5 volts is the setting to use and that I should adjust the apms. with the size of the part I am plating. Is there any reason to adjust the voltage?

By the way I am going to plate some parts for a 1973 Porsche 911 2.4S.

Thanks guys

John