Hi,
I just did some parts with flash copper then copy chrome. After they came out of the copy chrome, they had a real bad yellow tint to them. I plated 20sq. in. at .61 amps for an hour. I was able to polish them afterwards with white compound/sewn cotton wheel, and they looked good, but i've never had to do that before. any help would be great thanks!!
Woody
|