Re: Experimenting with paint and powder
Well that's a whole lot better than I could have done...I'm thinkin it looks pretty good. I have, however seen a few coaters that have powdered the base, air brushed, then powdered the clear. I would have thought that the paint would have bubbled up. I don't know what type of paint was used but it did come out looking mighty nice.
|