Quote:
|
With my plastic bucket insulated , even after 2 hrs, my cad. solution won,t go part 95 degree,s with a single heater, anybody else seeing this problem??
|
Yes. See this previous discussion:
copy cad power problems
I'm using a 200w aquarium heater in a 3 gallon NON-insulated tank and have no problems getting to 100º+. Your heater is either too small, or defective.
Quote:
|
Im being told a Porcelain pot is better to use?? true??
|
Also discussed in the above discussion. The zinc electrolyte is an acid, it may react w/porcelains, but I don't know for sure. Stick w/the recommended plastics.
Quote:
Also abody know the shelf life of the cad solution sitting
|
My original formula is 2 1/2 years old and still working good.