Hey Jim!
Thanks for the info. It was the first batch I had done in a very long time. (I have been doing much more powder coating these days) I double filtered all of my solutions because they had been sitting around. Then I added more brightener. I ran the copy chrome at right around 70 degrees, so i don't think it could be too hot. Too close maybe. Also the anode definitely might have been dirty. They too had been sitting around oxidizing. I will say that might second batch came out better with less yellowing. Both batches polished up real nice and shiny. I just hope they stay that way, and the parts don't yellow much later on. Hopefully, I'll be back in full plating swing (along with the powder) real soon. The only real problem is finding time. Anyone know where to get more of that?