Default Re: Copy Cad with heaters, Temp. up past??

Quote:
Originally Posted by MrPontiac
may i ask, how long does it take your 200w heater to get your temp up to 100 degree,s??
Depends on how cold the electrolyte is to begin with.

My workbench is in an unheated basement. In the summer, when it's 90º outside, the basement is 70-75º. Takes about an hour to get it to 105º.

In the winter, below freezing outside, the basement is about 45º. With the old formula, it took about an hour to get it to 70º.

Haven't used the new formula in winter yet, but from the above, I'd say about 2 hours to go from 45º to 100º.

Sean