Re: Vibratory Polisher Pro's & Con's
thanks for your help, (i didnt realise caswell sold them), the parts i would be doing would not fit in the round type as most of the parts are between 2ft and 2ft 6" long (rocker covers, cam belt covers, mainfolds etc...) so i would be looking at a tub type around 3 ft x 1 ft x 1ft = 3 cubic ft (i think lol), the media seems to be a reasonable price if it can be re-used so that shouldnt be a problem, the run times of each media seems ok,
so now i need to know roughly how much media is needed for a 3 cubic feet tub (does 65 lb's sound about right ?) and is there anywhere i can find close up pictures of work done by vibratory polishers to get an idea of the finish i can expect, also will they distort mating surfaces ? would the mating surface need skimming afterwards (for example where the manifold fits to the engine block) or would it take an even amount off all over ?.
Last edited by daz2206; 11-22-2006 at 09:23 AM.
|