Quote:
|
Originally Posted by mpierich
The specks are probably either small pores or inclusions of impurities. Look at them with a magnifying glass.
With this problem I always go slower in speed rather than faster. It makes a big difference without the fibers slapping the metal so hard. But I still think the white rouge finish is dandy.
|
I think you are right. I did notice that slower seemed to make a difference in makin a better finish. I agree that the white is great and that is what i will end with but I was just tryin to find an answer to why the red is causing a problem. Just weird that the interior trim has these specks but the exterior trim comes out flawless. Well thanks for all the input guys.
thanks