Im running 1.5 amps on my rectifier, parts are 3/16 tube only 1/4 long.
And how many of these parts are you plating at the same time?

3/16 x 1/4 tube is < .3 sq-in surface area (inside & out). 1.5 amps is enough to plate 37 of them at a time.

Are doing 37 parts at a time? If not, then you're using too much current and burning them.