I have a 3cu MR DEBUR for ceramic coating polishing with 3mm-4mm mix of ceramic balls
and it works great with the right soap
and I have a small 12" inch bowl with walnut and meta polish for small parts
and it also works good
but a buffing is need for a very high chrome like finish
still the tumblers reach areas where anything else won't work.