Re: Ruff sandpaper like finsh??? Zinc??
I don,t know, there not burning at all but they are plating ok, its just looks like sandpaper finish, gritty, ive tryed again down to .7 amps and im still getting this finish a little ruff. Sort a dumb question?? ok?? i trimmed my anode plates like the book says but there sitting in the bucket lope sided i have the outside strip hanging over the bucket like a hook. Are you doing this also?? Also, may i ask, how are you jumping from one anode to the other for the + field?? I just bought a jumper wire with 2 aligator clips on it, is this what the norm is??
|