Default Re: having problems !!!!

I soak the piece in the degreaser for about 5 min, rinse in distilled water,then in the pickle #4 for a few min, rinse(distilled) then in the flash copper for 15 min, rinse(distilled) and then in the copy chrome for 15 min.
The copper comes out good but the chrome is bad. Yesterday when I was giving this a try I noticed that at times there was no voltage reading on the rectifier but it showed amps., and then both needles were jumping up and and down. I checked my connections they seem to be fine. Was wondering if there might be a problem witht he rectifier. I hve ordered the PH tester. I just cant believe that the PH would be out of balance already. If the Copy chorme gets to hot will it demish the chrome brightener? The one angle that I did came out dark almost antique looking and I was at 1/2 amp.
Thx
toddtracb