Thread
:
Powder Coating Eyeglass frames
View Single Post
#
3
(
permalink
)
11-28-2006, 09:47 AM
bzer1
Experienced Metal Finisher
Join Date: Jan 2004
Posts: 277
Re: Powder Coating Eyeglass frames
The biggest problem I can see is the hinged ear pieces might get coated open. If you can get past that it shouldn't be a problem.