Default Re: Powder Coating Eyeglass frames

the hinge didn't gave me much of a problem
I cut a line with a hobby knife and fix it
and I also did it at 100Kv so the coat was thin a thicker coat might be a problem.
real problem was placing the glass back
coating got inside the groove area where the glass rests
and the glass didn't fit
had to scratch the groove with the hobby knife
for my second frame I taped the groove and worked .