Default Re: Acid pickle renoving rust?

Thanks Lance

I have a copy of the page in the manual (was not in my manual) that was sent to me from Caswell Europe yesterday and there is no question about it, the manual says to mix batteryacid in the yellow chromate crystals and water. Mr. Jeep also told me in the mail he sent me.

From their mail to me:

Page 103 of the manual describes the approach to using the Yellow Chromate. You have not put the sulphuric acid in and so it cannot etch on the zinc.

Who is right?

best
John