just got my first sisal wheel from caswell and im having a little trouble, when i switched on the buffer with the new sisal wheel lots of sections started to release the fibers (like weeds growing out of a grass field), also i could not get the emery compound to stick to the wheel it just took a big section of the compound bar in seconds.

can someone tell me what i need to to or what im doing wrong.