Default Re: Need help with first real job estimate

Ya, I would estamate $10 for the larger parts, $5 for the smaller ones. Overall cost of approx $250=270 fro teh works. They're pretty easy to do, but the looks. Clean and shoot. Might want to do a Zinc Phostphate coating first, to help with adheasion. Metal parts like that I just moisten a rag with Caswells Zinc Ph concentrate and wipe teh part. Just enough to moisten it. Then let part dry. Will help with long term adhesion and corrosion resistance