New 30-50 KV gun does not work.
I just got my new gun and there is no power out put.
I checked the fuse and it's OK. The foot switch appears to work because the "in use" light lights up when peddle is depressed. When tip is touched to the ground there is no arc. I also used an ohm meter between the tip and ground and got no reading when the peddle was depressed.
Any ideas?
I haven’t called Caswell because it’s too late.
BTW I'am well versed in how these units work so I'm sure it's not me.
|