Re: black chrome problems
Looks like fisheyes (contaminents such as oil), but it's hard to tell from the pics. If the chrome didn't do it then maybe something is getting onto the surface between coats. Moisture in your lines will cause this too, and candies will do it worse than solids. Try being extra careful keeping the surface clean and a moisture filter right at your gun. If you have one already change it and try that.