hey bandit nice work, if you have trans gold maybe you want to try that over lolly red as a test , i did near chrome then lolly red then candy gold over then i compare with near chrome and lolly red only . a bit darker looks deeper candy with a very slight gold tint when viewed from an angle . it s close to liquid paint red candy over gold base , i coudn t get a picture but i ve showed the sample to couple of customers nd they really liked it