Have you tried spraying the black chrome separately?

Like chromeitout said, from the pictures the defects do look like fisheyes. Another contamination source might be from traces of incompatible powder in your booth, or in the powder itself.

Back ionization or poor grounding, like Jtagger19 mentioned, could also cause similar defects, but then your bottom layer would also show the spots.