Re: advise needed
Either kit will provide a lasting finish if the items are processed correctly. The advantage to copy chrome is that it requires less amperage per square inch than chrome. The chrome kit will give you the chemicals necessary to plate onto plastics except for the conductive paint. Once the part is painted it needs to be immersed in the acid copper for at least 15 minutes before plating with either nickel (then chrome) or copy chrome.
|