Originally Posted by daz2206
ok, i had a go at another cambelt cover and it seems to have come out ok this time, i didnt put it in the oven first because i didnt know how hot to make it, i think i must have done something wrong the first time around.
Nice! You oughta try to figure out what you did differently...