View Single Post
  #4 (permalink)  
Old 12-16-2006, 06:10 PM
btorres09 btorres09 is offline
Newbie
 
Join Date: Dec 2006
Posts: 7
btorres09 is on a distinguished road
Default Re: Help Polishing GSXR 1000 subframe

thanks for the reply guys...im working on getting a pic...but they look like veins....im new at this so i have never seen anything like that....the only thing i have polished so far is a heel guard with no problems...another question. after using emery/sewen,then brown/ canton, then red/ sewen, then white/ loose i can see my reflection but for some reason it looks dull and dark....
Reply With Quote